ISSN 0862-5468 (Print), ISSN 1804-5847 (online)

 Basic Information
Home
Publisher
Editorial board
Editors
Impact factor

Online submission
Author guidelines
Instruction for reviewers
Download instructions
 List of Content
Volume 55, 2011
  - Issue 1
  -
Issue 2
  - Issue 3
  - Issue 4
Volume 54, 2010
  - Issue 1
  -
Issue 2
  - Issue 3
  - Issue 4
Volume 53, 2009
  - Issue 1
  -
Issue 2
  - Issue 3
  - Issue 4
Previous Issues
  - 1995 - 2008
 Search
Advanced Search

Ceramics-Silikáty 39 (1) 9-13 (1995)


LIQUIDUS TEMPERATURE AND STRUCTURE OF THE GLASS MELTS IN THE 15 Na2O.10 (MgO, CaO, Ti02, ZrO2).75 SiO2 SYSTEM

P. Šimurka, M. Liška, J. Antalík

The liquidus temperature in the 15 Na2O.10 (MgO, CaO, TiO2, Zr02).75 SiO2 glass system was measured. The data have been used for the indication of the structural role of Ti02 in this glass system. From the values of liquidus temperature the activity of Si02 in the melt was calculated according to Le Chatelier-Schreder equation. The analysis of liquidus temperature, based on the SiO2 activity coefficient evaluation indicates, that Ti4+ forms discrete anionic complexes with modifying cations.