Ceramics-Silikáty 40 (4) 131-136 (1996) 


EFFECT OF GRINDING OF Y2O3, BaCO3 AND CuO ON SYNTHESIS OF YBa2Cu3O7 

B. Plešingerová, A. Buchal, V. Šepelák, K. Tkáčová

The very fine and surface reactive powder mixture was prepared by highly intensive short time mill grinding of the components Y2O3, BaCO3 and CuO. Pure YBa2Cu3O7 created by reaction of the components of grinding mixture at temperature 900 - 950°C. The temperature of the synthesis of YBa2Cu3O7 decreased owing to the grinding about 50 to 100°C. Lower temperature of the synthesis had a positive effect on the purity of the final product.